Bath Make-Up

 OPTIMUM RANGE
E-Chrome Ultra Yellow Red A 10% by volume  9%-11% by volume
E-Chrome Ultra Yellow Red B 10% by volume  9%-11% by volume

 

Step by Step Application
Chromating on zinc-plating surfaces with E-Chrome Ultra Yellow Red is accomplished as follows:

  1. Zinc plate parts to .0003. The brightness of the final finish will be directly related to the brightness of the plated surfaces.

  2. Cold water rinse

  3. 1% by volume Sulfuric Acid, rinse to neutralize residual plating solution

  4. Cold water rinse

  5. Immersion in E-Chrome Ultra Yellow Red solution for the length of time required to produce the desired finish.

  6. Cold water rinse

  7. Hot Air Dry – 150° F

Operating Conditions

 OPTIMUM RANGE
pH*:1.8 1.65 – 2.0
TEMPERATURE:120° F (54°C)  90°-150°F (32°-66°C)
TIME:1 minute  30 seconds – 5 minutes
AGITATION:Air agitation may be helpful in rack situations

* Lower pH with E- Chrome Ultra Yellow Red A and B; raise pH with Ammonium Hydroxide